Applications
Formulated specifically for use when changing the static port heater element on the DC-9 and MD80 powerplants
Once the silicon resin and aluminum powder are thoroughly mixed and applied to the substrate, AP 280 will thicken to a “putty-like” consistency
Mix both components of AP 280 completely prior to applying it to an area
Use spatula to apply non-curing and pressure sensitive putty/aluminum mix at about 15 mils (381 microns) thick
Let mix stand for 1 to 2 hours so that it gains “tack”
Manipulate mix to lay heater element into putty compound